The fracture behavior and fracture manner in the diffusion-bonded joints were elucidated by macro fracture and magnified surface morphologies. The macro fracture morphologies (flat fracture) exhibit which the propagation of crack transpired along the MEA/DD5 interface in tensile tests on the joints obtained at 1020, 1050, and 1080 °C (Figure 8a–